Table 3

Mechanical properties of wear-resistant coatings.

Coating , GPa σ0, MPa E, GPa σt, GPa KIC, MPa·m½ KICP, MPa·m½
TiN 29.16 −775 307 9.53 3.39 12.29
TiAlN 38.65 −1256 369 12.26 4.07 14.77
TiZrN 38.39 −902 379 12.38 4.22 14.44

− microhardness, σ0 – residual compressive stresses, E − modulus of elasticity, σt − yield strength, KIC − critical stress intensity factor, KICP − fracture toughness.